Technical guide

Cold galvanizing: definition, products, preparation, uses and limits

Hicham M, P Eng, PMP8 min read

Related solution: Cold Galvanizing & Metallizing

Cold galvanizing is the application of a zinc-rich paint, by brush, roller or spray, on prepared steel. Once dry, the film holds enough metallic zinc to protect the steel galvanically, with no molten zinc bath. It is done on site, on installed structures, and its performance depends mostly on surface preparation and on the thickness applied.

The term is misleading: this is not galvanizing in the metallurgical sense, it is a coating. It is nevertheless the usual way to protect or touch up steel that cannot be sent to a galvanizing plant. This guide is written for maintenance managers and industrial project managers in Quebec and Ontario. Induscoat works on industrial and commercial assets only, not on residential jobs.

What exactly is cold galvanizing?

Cold galvanizing is a coating made of zinc dust dispersed in a binder and applied at ambient temperature. After drying, the zinc particles touch each other and touch the steel: zinc, being more anodic than steel, corrodes in its place at scratches and holidays.

Two binder families exist:

  • Organic binder (most often epoxy). More forgiving to apply, easy to overcoat, and used as the primer in most paint systems.
  • Inorganic binder (silicate). It gives a hard film with very good abrasion and heat resistance, but it demands stricter preparation and curing conditions.

Our comparison of inorganic vs organic zinc primer covers that choice in detail. The position of zinc relative to steel can be read in the galvanic series table, and the zinc-rich primer glossary entry sums up the vocabulary.

How much zinc must the dry film contain?

The dry film must hold enough zinc for the particles to stay in electrical contact with each other and with the steel; below that threshold, the product is just a grey paint with no galvanic effect. The value that matters is the one on the product data sheet, stated as the proportion of zinc in the dry film, not in the can.

Three references frame this requirement, without anyone having to memorize a single figure:

  • SSPC-Paint 20 classifies zinc-rich paints by binder type and by the level of zinc dust in the dry film.
  • ISO 12944-5 sets a minimum zinc dust content for a primer to be called zinc-rich within a paint system.
  • ASTM A780 describes the repair of damaged areas on hot-dip galvanized coatings, including with zinc-rich paint, and states the content expected in the dry film.

In practice, ask the supplier for the data sheet and check three lines: the zinc content of the dry film, the standard the product claims to meet, and the recommended thickness per coat. A product that does not state its zinc content in the dry film has no place in an industrial specification.

Aerosol or industrial system: what is the difference?

An aerosol is for spot touch-ups; an industrial system is for protecting an asset. The difference lies in the thickness deposited, the zinc content, the preparation required and the inspection that is possible.

CriterionZinc aerosolIndustrial zinc-rich system
Intended useTouch-ups on small areas, welds, cut edgesStructures, equipment, tanks, large surfaces
PackagingSingle-component, ready to useOne or several components, mixed and kept under agitation
Thickness per passLow, several passes neededData sheet thickness reached in one or two coats
Zinc content in dry filmVaries by product, check the data sheetDeclared to SSPC-Paint 20 or ISO 12944-5
PreparationOften power tool, localAbrasive blasting to the specified grade
InspectionVisual, sometimes a thickness readingProfile, ambient conditions, thickness, records
OvercoatingRarely plannedPart of an epoxy and polyurethane system

An aerosol sprayed over rust or over a wire-brushed surface gives a grey colour, not galvanic protection. For touch-ups on galvanized parts, the method is in our article on field galvanizing repair to ASTM A780.

What surface preparation is needed?

The steel must be clean and rough, because zinc has to touch bare metal to protect it. The preparation grade comes from the data sheet and the specification: most often abrasive blasting to SSPC-SP 10 for an inorganic zinc, and at least a commercial grade for many organic zincs.

The sequence matters as much as the grade:

  • Degreasing. Oil and grease are removed before blasting (SSPC-SP 1), otherwise the abrasive spreads them.
  • Blasting. Abrasive blasting removes mill scale, rust and old paint and creates the required surface profile.
  • Local touch-ups. Where blasting is not possible, power tool cleaning to bare metal such as SSPC-SP 11 may be accepted by the data sheet for small areas.
  • Ambient conditions. The surface must stay above the dew point, and the delay between blasting and application must stay short.

Zinc-rich paint is not applied over old paint: it would lose contact with the steel. The application itself (mixing, agitation, thickness, curing) is described in our zinc-rich primer application guide.

When is cold galvanizing used?

It is used whenever steel needs zinc protection and cannot go through a bath. The most common cases in a plant are these:

  • Assets in place. Structural frames, walkways, pipe supports, handrails and equipment that will not be dismantled.
  • Parts too large or too thin for the kettle. Large welded assemblies, sheet that would distort with heat.
  • Touch-ups on hot-dip galvanizing. Field welds, cuts, drilled holes and handling damage.
  • Primer of a paint system. First coat of a system defined to ISO 12944, overcoated with an epoxy and a topcoat.
  • Zone maintenance. Restoring the corroded areas of a structure without redoing everything.

In all these cases, cold galvanizing is part of a protective coatings system chosen for the environment: dry interior, industrial atmosphere, coastal exposure, de-icing salts.

What are the limits of cold galvanizing?

Its main limit is that it remains a coating: it has neither the metallurgical bond nor the mechanical resistance of hot-dip galvanizing. It protects well when applied by the book, and poorly when preparation is skipped.

  • Dependence on preparation. Without bare metal and a profile, the film neither adheres nor protects.
  • Thickness to watch. Too thin, the zinc reserve runs out quickly; too thick, some products crack. The range comes from the data sheet and is measured as dry film thickness.
  • Unfavourable environments. Zinc is consumed quickly in acidic or highly alkaline conditions; for immersion, the product choice is validated with the manufacturer.
  • Impact and abrasion. An organic zinc resists impact less than a hot-dip layer.
  • Appearance. The finish is matte grey; a topcoat is needed for colour and, in aggressive environments, for durability.

No service life can be promised without knowing the environment, the thickness and the full system.

How does it differ from hot-dip galvanizing?

Hot-dip galvanizing immerses the part in a bath of molten zinc, at the plant, and forms zinc-iron alloy layers bonded to the steel (ASTM A123, ISO 1461). Cold galvanizing deposits a film of zinc-rich paint, on site, mechanically bonded to the surface.

Hot-dip suits new, removable parts that fit the kettle: it also protects the inside of hollow sections and stands up very well to handling. Cold galvanizing suits installed assets, oversized parts and touch-ups. Between the two, metallizing sprays molten zinc onto blast-cleaned steel. Our comparison of cold galvanizing vs hot-dip gives the full decision table, which we do not repeat here.

How do you get cold galvanizing done in a plant?

Start by describing the asset and its environment, then set the preparation grade, product, thickness and inspections before discussing the schedule. Our cold galvanizing service covers preparation, application of the zinc-rich system, the following coats and the inspection records.

Our crews and qualified subcontractors work out of LaSalle, in Montreal and across Quebec and Ontario. Send photos, dimensions, the service environment and the current condition of the steel through the request a quote form: pricing on consultation, reply within 24 business hours.

Frequently asked questions

Is cold galvanizing as durable as hot-dip galvanizing?

Not at equal thickness and conditions: the hot-dip layer is metallurgically bonded to the steel and resists impact better. A zinc-rich system that is well prepared, overcoated and maintained still gives lasting protection on an asset in place.

Can cold galvanizing be applied over rust?

No. Zinc must touch bare steel to work. Rust, mill scale and old paint are removed first, to the grade stated on the data sheet.

Does cold galvanizing need a topcoat?

It depends on the environment. In a dry interior, zinc alone can be enough. In industrial, marine or salt-exposed atmospheres, a compatible intermediate coat and topcoat extend the protection.

Is a zinc aerosol enough to touch up a galvanized part?

Yes for small areas, provided the product states its zinc content in the dry film, the surface is prepared to bare metal and the thickness required by ASTM A780 is reached, which often takes several passes.

#cold galvanizing#zinc-rich paint#zinc#corrosion protection#steel structures
HM

Hicham M, P Eng, PMP

Engineer and project manager (PMP) at Induscoat. Over 16 years of experience in industrial coatings, composite repairs and wear protection on mining, energy and petrochemical sites in Canada and internationally.