Home/Regions/Mauricie and Centre-du-Québec
Québec · Canada

Industrial coatings and maintenance in Mauricie and Centre-du-Québec

Induscoat works in Mauricie and Centre-du-Québec from LaSalle, Montreal, for chemical plants, aluminum facilities, paper mills and the industrial parks of Trois-Rivières and Bécancour: protective and anti-corrosion coatings, tank and secondary containment linings, cold repair and epoxy grouting of machinery. The St. Lawrence highway corridor makes pre-job visits and shutdown logistics straightforward.

Industrial parks along the corridor: chemicals, aluminum, paper

On the south shore, the Bécancour industrial and port park brings together chemical plants (chlor-alkali, hydrogen peroxide, hydrogen), an aluminum smelter, silicon production and a deep-water port open year round. On the north shore, Trois-Rivières, where the Saint-Maurice meets the St. Lawrence, was long a major pulp and paper centre and still has an active port and industrial parks. The Saint-Maurice valley also has hydroelectric plants and metallurgy and metal processing facilities.

Failure modes follow these processes. In chlorine, acid and caustic chemistry, steel, containment and floor concrete, vessels and piping suffer direct chemical attack. At the smelter and in silicon production, it is heat, abrasive dust and an industrial atmosphere. In paper mills, it is constant humidity and process liquors.

Climate, classified areas and shutdowns in the St. Lawrence valley

The St. Lawrence valley climate is milder than in northern regions, but freeze-thaw cycles are frequent and humidity near the river stays high. Meltwater, process splash and de-icing salts around loading docks and access roads keep structures corroding and concrete degrading.

In chemical plants, classified areas and the products on site require strict permits: limited hot work, gas detection, confined space. Cold bonding repairs and flame-free coatings meet those constraints. The reasonable distance from Montreal allows a site visit before quoting and simple mobilization once the shutdown window is set.

Services for the region's plants

Containment basins and slabs around chemical tanks receive coatings chosen for the product, its concentration and temperature; concrete is repaired and prepared before application. Tanks and process vessels are lined internally for the stored product, with holiday testing. Above-ground piping and supports, often attacked at contact points and under insulation, are treated and repainted.

On the mechanical side, corroded heat exchangers, pumps and flanges are repaired cold, and rotating machinery is epoxy grouted on its foundation. Corrosion-resistant custom parts are made to drawing or reproduced by measuring the existing part.

Standards required in specifications

In the corridor's chemical and metallurgical plants, specifications commonly require an ISO 12944 system for steel, surface preparation to ISO 8501-1 or SSPC/AMPP, API 653 for above-ground storage tanks and API 570 for process piping when the owner follows those codes, and API RP 686 for machinery grouting.

For coatings in contact with chemicals, compatibility is checked on the manufacturer's data sheet for the actual product, concentration and temperature. The QC file records preparation, film thickness, adhesion and continuity.

Regions served

  • Trois-Rivières and Cap-de-la-Madeleine
  • Bécancour and its industrial and port park
  • Shawinigan and the Saint-Maurice valley
  • La Tuque and Haute-Mauricie
  • Drummondville and Victoriaville
  • Nicolet and the south shore of Lac Saint-Pierre

Industries served

  • Chlor-alkali and industrial gas chemistry
  • Aluminum and silicon
  • Pulp and paper
  • Metallurgy and metal processing
  • Hydroelectric generation
  • Trois-Rivières and Bécancour ports

Services & solutions

  • Secondary containment and slab coatings
  • Internal linings for tanks and process vessels
  • Corrosion protection for piping and supports
  • Cold repair in classified areas
  • Epoxy grouting of machine foundations
  • Corrosion-resistant custom parts

Brands distributed

  • Induscoat — own brand (Canada coatings)

Operational mobilization

In Mauricie and Centre-du-Québec, a site visit usually comes before the quote. Mobilization follows the plant's shutdown window, with the permits and health and safety plans required: confined space, hot work, classified areas, gas detection. Outdoors, substrate temperature and dew point decide what can be applied.

Frequently asked questions

Do you work in the Bécancour industrial park?

Yes, from LaSalle, for planned shutdowns and maintenance work. We follow each plant's own access, permit and health and safety rules. Induscoat has no facility in Bécancour.

Which coating suits a chemical containment basin?

It depends on the product contained, its concentration, its temperature and the expected contact time in a spill. Novolac epoxies and vinyl esters cover most acids and bases; the manufacturer's data sheet confirms compatibility. Concrete must be dry, sound and prepared before application.

Can equipment in a classified area be repaired without hot work?

Often, yes. Metal-filled composites and polymers cure cold and need neither flame nor welding. They are used to rebuild flanges, pump and valve bodies and thinned walls, within the pressure and temperature limits set by the owner.

Do you cover Drummondville and the rest of Centre-du-Québec?

Yes. Drummondville, Victoriaville and the region's industrial parks are served from LaSalle, as is Mauricie. For the rest of the province, see the Quebec page.

A project in Mauricie or Centre-du-Québec?

Send the data sheet for the product in contact, photos and dimensions: we propose the system and arrange a site visit if needed.

Induscoat is the Quebec-Ontario subsidiary of Induscoat Group, an industrial group active in Canada and Morocco.