Technical guide

Zinc metallizing: step-by-step process, cost factors and service life

Hicham M, P Eng, PMP7 min read

Related solution: Thermal Spray Metallizing (Zinc, Aluminum, Zinc-Aluminum)

Zinc metallizing melts a zinc wire, with an electric arc or a flame, and sprays it with compressed air onto abrasive blast-cleaned steel. The droplets lock onto the surface profile and build a zinc layer that protects the steel as a barrier and galvanically. It is done in the shop or in the field, and is then sealed.

It is also called zinc thermal spray or zinc spray metallizing. The process interests owners who want zinc protection on an asset that is too large for a galvanizing kettle, or already installed. This guide follows the job in order, for maintenance managers and project managers in Quebec and Ontario. The choice of metal (zinc, zinc-aluminum or aluminum) has its own article: zinc vs aluminum thermal spray.

How does zinc metallizing work, step by step?

Metallizing always follows the same sequence: prepare, verify, spray, measure, seal. Each step has its own check, and none can be made up for at the next one.

StepWhat is doneAssociated check
Asset reviewSurvey of surfaces, access, edges and welds to dressList of areas, photos, governing specification
Protection and maskingProtecting nearby equipment, masking bearing seats and threadsVisual check before blasting
DegreasingRemoving oil and grease (SSPC-SP 1)Visual examination
Abrasive blastingAngular abrasive, SSPC-SP 5 or SSPC-SP 10 per the specificationCleanliness, surface profile (ASTM D4417), residual dust
SprayingCrossed passes, constant distance and angleAmbient conditions, time since blasting
MeasurementLayer thickness with a non-destructive gaugeSampling plan of the standard, records
SealingLow-viscosity sealer applied soon after sprayingAppearance, timing, compatibility
Optional topcoatCompatible paint systemDry film thickness, recoat windows

The two working references are ISO 2063, for thermal-sprayed zinc, aluminum and their alloys, and the joint standard SSPC-CS 23.00 / AWS C2.23, which covers preparation, application, sealing and inspection. The specification states which one governs.

What equipment does zinc metallizing require?

It takes two complete stations: a blasting station and a spray station, both fed with clean, dry compressed air. Air quality matters as much as the gun: oil or water in the air contaminates the steel just before spraying.

  • Electric arc spray. Two zinc wires are fed into the gun, an arc melts them and an air jet atomizes the metal. It is the most common process on large surfaces, because of its deposition rate.
  • Flame spray. A wire is melted by a fuel gas and oxygen flame, then atomized. The equipment is lighter, useful for small areas and touch-ups.
  • Blasting. Blast pot, angular abrasive, properly sized compressor, dryer and filters. See our abrasive blasting service.
  • Collection and containment. Dust collector, tarps or an enclosure depending on the site, to hold back abrasive and metal fume.
  • Operator protection. Supplied-air respiratory protection, hearing protection and protection from arc radiation. Zinc fume calls for ventilation and exposure control.
  • Instruments. Calibrated thickness gauge, profile measuring equipment, hygrometer and surface thermometer, pull-off adhesion tester.

Shop or field: where is metallizing done?

In both places: in the shop for new or removable parts, in the field for installed assets. The choice depends on part size, whether it can be transported, and the shutdown window.

In the shop, ambient conditions are controlled, the abrasive is recovered and the delay between blasting and spraying stays short. Parts are then handled with care, and erection joints and field welds are completed on site.

In the field, metallizing avoids dismantling: structures, tank interiors, penstocks, gates, decks. In return it requires containment, waste management, sometimes heating or dehumidification, and tight coordination with operations. The constraints of working inside a plant are described in our article on blasting in operating plants and dust control.

In both cases, preparation decides the outcome. Cleanliness grades are explained in our NACE 2 / SSPC-SP 10 surface preparation guide, and surface profile is defined in the glossary.

What factors move the price of metallizing?

Price depends first on preparation and access, well before the zinc itself. No figure per square foot means anything without knowing the asset; the factors below explain the gap between two quotes.

  • Area and geometry. Flat plate goes faster than lattice, angles or a baffled tank interior.
  • Starting condition. New steel with mill scale, thick old paint, deep rust or lead paint: blasting time changes severalfold.
  • Preparation grade required. White metal takes more time and abrasive than near-white.
  • Zinc thickness specified. It sets the amount of wire and the number of passes.
  • Sealer and topcoat. A duplex system adds coats and waiting times.
  • Access and containment. Scaffolding, lifts, enclosure, ventilation, confined space work.
  • Location and schedule. Shop or field, planned shutdown work, night shifts, mobilization distance.
  • Inspection and records. Frequency of readings, adhesion tests, third-party inspection.

These factors are detailed, still without figures, in our article on thermal spray metallizing cost. The calculation over the life of the asset uses the coating total cost of ownership method.

How long does zinc metallizing protect steel?

Service life depends on three things: zinc thickness, how aggressive the environment is, and whether a sealer or topcoat is present. Zinc is slowly consumed as it protects the steel; the thicker the layer and the milder the environment, the longer the reserve lasts.

ISO 2063 links recommended thickness to the environment category and the intended durability; that is the reference to cite in a specification, instead of a promise in years. Three points weigh on the result:

  • The environment. A rural atmosphere uses up little zinc; a marine atmosphere, de-icing salts or acidic conditions use it up quickly.
  • The sealer. It closes the porosity of the layer and delays its consumption.
  • The duplex system. Paint over metallizing protects the zinc, which protects the steel: the two lifetimes reinforce each other.

Poorly prepared metallizing does not age: it comes off. That is why the profile, thickness and adhesion records are worth as much as the layer itself.

What maintenance does metallizing need?

It needs little maintenance, but regular maintenance: planned visual inspections, cleaning of deposits and local touch-ups before the steel is reached.

  • Inspection. Look for red rust at edges and connections, chalking or wear of the sealer, and mechanical damage. White zinc corrosion products show that the layer is working, not that it has failed.
  • Cleaning. Salt deposits, process dust and water traps are removed, because they speed up zinc consumption.
  • Renewing the sealer or topcoat. This is done when the film is worn, before the zinc is widely exposed.
  • Touch-ups. The area is prepared to the required grade, then receives sprayed zinc again or, where the specification allows, a zinc-rich paint.

A coating maintenance and inspection program sets the frequency of visits according to the environment.

How do you get a quote for zinc metallizing?

Describe the asset, its environment and the work window; the rest is settled at the site visit. Our thermal spray metallizing service covers preparation, spraying, sealing, topcoating and the inspection file, as part of a protective coatings system suited to the environment.

Our crews and qualified subcontractors work out of LaSalle, including in Saguenay-Lac-Saint-Jean, on the Côte-Nord and in Ontario. Send photos, dimensions, the service environment and the specification if one exists through the request a quote form: pricing on consultation, reply within 24 business hours.

Frequently asked questions

Does zinc metallizing replace hot-dip galvanizing?

It replaces it when the part cannot go to the kettle: an installed asset, a part that is too large or sensitive to heat. For new parts that fit the kettle, hot-dip galvanizing is often simpler.

Can zinc metallizing be done on site, without dismantling?

Yes. That is one of the main advantages of the process. Plan for containment, dust and fume collection, and ambient conditions that meet the standard.

Should zinc metallizing be painted over?

A sealer is almost always recommended. A topcoat is added for colour or for aggressive environments, using a compatible system named in the specification.

What zinc thickness should be sprayed?

The one set by the project specification and by ISO 2063 or SSPC-CS 23.00 / AWS C2.23 for the environment and the intended durability. It is measured and recorded during the job.

#metallizing#zinc#thermal spray#corrosion protection#steel structures
HM

Hicham M, P Eng, PMP

Engineer and project manager (PMP) at Induscoat. Over 16 years of experience in industrial coatings, composite repairs and wear protection on mining, energy and petrochemical sites in Canada and internationally.

Related articles

Comparison

Zinc, zinc-aluminum or aluminum metallizing: which to choose?

Metallizing deposits a layer of zinc, zinc-aluminum alloy or aluminum on steel. This guide explains which metal to choose by environment (atmosphere, immersion, seawater, temperature), the preparation required, the role of sealer and topcoat, and the ISO 2063 and SSPC-CS 23.00 / AWS C2.23 standards.

Hicham M, P Eng, PMP
7 min
Economics

Thermal spray metallizing cost: the 8 factors behind the price of zinc or aluminum spraying

The cost of thermal spray metallizing with zinc, aluminum or zinc-aluminum alloy depends on eight measurable factors. This guide explains how each one weighs, how to compare two quotes and what to provide for an accurate price.

Hicham M, P Eng, PMP
7 min
Comparison

Cold galvanizing, hot-dip galvanizing or metallizing: which to choose?

Hot-dip galvanizing, cold galvanizing and zinc metallizing all protect steel with zinc, but not under the same conditions. This comparison explains how each works, its standards and its limits, then gives a decision table to choose by part and by site.

Hicham M, P Eng, PMP
7 min
Technical guide

SSPC-SP10 surface preparation (NACE No. 2): the near-white metal blast guide

SSPC-SP 10/NACE No. 2 is the near-white metal blast grade specified for most immersion and severe-service coatings. This guide gives the exact definition, compares it with SP 5, SP 6 and the rest of the SSPC family, and covers what the standard leaves to the specification: profile, salts, dust, dew point and time to primer.

Hicham M, P Eng, PMP
10 min