Industrial painting and coatings in Sudbury
Induscoat applies protective coatings, wear-resistant coatings, rubber lining and industrial paint to concentrators, conveyors, chutes and tailings facilities in the Sudbury mining basin. We have no office in Sudbury: our mobile crews travel from LaSalle, Montreal, on a trip planned with the site. Send photos and dimensions and you receive a quote within 24 business hours.
What we do in Sudbury
We protect steel and concrete in Sudbury mining and metallurgical facilities against abrasion, corrosion and process chemicals: abrasive blasting, wear-resistant coatings for chutes and hoppers, rubber lining for tanks and slurry piping, mining equipment and structure painting, and tank linings. Work is carried out by our crews and qualified subcontractors, under one quote and one inspection file.
Coatings are our core business. The system is chosen from ore particle size and velocity, process water chemistry and ISO 12944 corrosivity, then applied to the manufacturer's data sheet.
Industrial sectors in Sudbury
Greater Sudbury lives around its nickel and copper basin, one of the largest mining districts in the world. Underground mines, concentrators, smelters, refineries and tailings facilities sit side by side, with a whole network of mining suppliers and service shops.
Each step wears steel down differently. At the concentrator, abrasive slurry eats through chutes, pump boxes, cyclones and piping. Conveyors and their galleries take impact, dust and moisture. Near smelters and refineries, gases and acid condensate attack structures. At the tailings, lines and concrete structures work in abrasion and immersion.
Most requested services in Sudbury
Rubber lining comes up often for flotation cells, pump boxes and fine slurry piping, where it absorbs abrasion better than a rigid film. For high-impact chutes and hoppers, a ceramic-filled wear coating applied at high build is usually the better choice.
Mining equipment painting covers conveyors, frames, galleries and concentrator structures. Hydro blasting removes hardened deposits and old films without abrasive. Reagent and process water tanks need an internal lining chosen for the liquid.
On-site work during shutdowns
We have no shop in Sudbury: our crews arrive with mobile blasting, painting, dust collection and heating units and work in place on your chutes, cells and structures. For a removable part, the site's maintenance shop or a local shop can serve as the work area if containment and ventilation are set up.
Wear work is mostly done during concentrator shutdowns. It is prepared so each part is ready, measured and coated within the planned window, with cure time included before return to service.
Travel, access and safety in Ontario
Sudbury is a real trip from LaSalle, by road into Northern Ontario. The window is set with the site first, then everything is settled remotely: survey from your photos and drawings, product quantities, abrasive, scaffolding and the operator's permits (confined space, lockout, work at height, underground work). Equipment arrives before the crew.
In Ontario, our work follows Ontario occupational health and safety rules for mines and construction projects, on top of the site's own rules. Jobs can be grouped with Timmins on one trip. Our project management service coordinates coatings with the other trades.
Climate in Northern Ontario
Sudbury winters are long and cold, and every product has a minimum application and cure temperature. Rubber and wear-resistant epoxies need a clean, dry, tempered substrate to bond. We work under heated, ventilated enclosures, with indirect heating, and measure substrate temperature, relative humidity and dew point before every coat.
Exterior work, such as conveyor galleries and tailings structures, goes in the warm season when possible. Inside the concentrator, slurry moisture causes condensation that has to be controlled even in summer.
Standards and inspection records
We apply the owner's specification. Common references are ISO 12944 for system selection, ISO 8501-1 and SSPC/AMPP standards for preparation (SSPC-SP 10 for immersion and wear service) and SSPC-PA 2 for dry film thickness. For rubber, hardness, adhesion and continuity are checked against the manufacturer's data sheet. The site receives a full file with photos.
Regions served
- Greater Sudbury
- Sudbury mining basin
- Onaping valley
- Northeastern Ontario
Industries served
- Underground nickel and copper mines
- Concentrators
- Smelters and refineries
- Tailings facilities
- Mining service shops
Services & solutions
- Rubber lining for cells and piping
- Wear coatings for chutes and hoppers
- Mining equipment and conveyor painting
- Abrasive blasting and hydro blasting
- Reagent tank linings
Brands distributed
- Induscoat, own brand (Canada coatings)
Operational mobilization
No permanent crew in Sudbury: every job is a planned trip from LaSalle, fitted to the concentrator shutdown, with survey, products, abrasive and permits prepared remotely.
Frequently asked questions
Do you have an office in Sudbury?
No. Induscoat has no office or shop in Sudbury. Our mobile crews travel from LaSalle, Montreal, on a trip planned with the site.
Rubber or ceramic for a chute?
Rubber handles fine particles and light impact well; ceramic-filled coatings stand up better to sliding coarse ore. The choice depends on particle size, impact angle and velocity.
Which safety rules do you follow in Ontario?
The Ontario occupational health and safety rules that apply to the site, plus the operator's internal rules and permits.
Can you line a cell in place?
Yes, during the shutdown, as confined space work, with ventilation, heating and site permits. Cure time is included in the window.
How much does your work cost in Sudbury?
Pricing is by quote. It depends on area, system, access, shutdown window and travel logistics. Send photos and dimensions: quote within 24 business hours.
Explore our solutions
A concentrator shutdown to prepare in Sudbury?
Send photos, dimensions and shutdown date: we prepare the system, products and trip from LaSalle. Quote within 24 business hours.
Induscoat is the Quebec-Ontario subsidiary of Induscoat Group, an industrial group active in Canada and Morocco.
Induscoat, the Group's Quebec-Ontario subsidiaryAreas we serve
- Industrial coatings and maintenance in Quebec
- Industrial coatings and maintenance in Montreal
- Industrial coatings and maintenance in Ontario
- Industrial coatings and maintenance in Abitibi-Témiscamingue
- Industrial coatings and maintenance on the Côte-Nord
- Industrial coatings and maintenance in Saguenay–Lac-Saint-Jean
- Industrial coatings and maintenance in Mauricie and Centre-du-Québec
- Industrial coatings and maintenance in Montérégie